Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

more free magazines
 
AISI 1026
Conditions Tensile Properties 
T (°C)Treatment
25 cold drawn (round bar (19-32 mm))  Tensile Strength (MPa) 490 
Yield Strength (MPa) 415 
Elongation (%) 15 
Reduction in Area (%) 40 
25 hot rolled (round bar (19-32 mm))  Tensile Strength (MPa) 440 
Yield Strength (MPa) 240 
Elongation (%) 24 
Reduction in Area (%) 49 