Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
 
AISI 1030
ConditionsImpact Energy (J)
T (°C)TreatmentMethodValue
25 annealed at 845°C   Izod 69.4 
25 normalized at 925°C   Izod 93.6 
25 rolled   Izod 74.6 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.