Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
 
AISI 1030
Conditions Tensile Properties 
T (°C)Treatment
25 annealed at 845°C   Tensile Strength (MPa) 463.7 
Yield Strength (MPa) 341.3 
Elongation (%) 31.2 
Reduction in Area (%) 57.9 
25 normalized at 925°C   Tensile Strength (MPa) 520.6 
Yield Strength (MPa) 344.7 
Elongation (%) 32.0 
Reduction in Area (%) 60.8 
25 rolled   Tensile Strength (MPa) 551.6 
Yield Strength (MPa) 344.7 
Elongation (%) 32.0 
Reduction in Area (%) 57.0 
25 water quenched, fine grained, tempered at 205°C   Tensile Strength (MPa) 848 
Yield Strength (MPa) 648 
Elongation (%) 17 
Reduction in Area (%) 47 
25 water quenched, fine grained, tempered at 315°C   Tensile Strength (MPa) 800 
Yield Strength (MPa) 621 
Elongation (%) 19 
Reduction in Area (%) 53 
25 water quenched, fine grained, tempered at 425°C   Tensile Strength (MPa) 731 
Yield Strength (MPa) 579 
Elongation (%) 23 
Reduction in Area (%) 60 
25 water quenched, fine grained, tempered at 540°C   Tensile Strength (MPa) 669 
Yield Strength (MPa) 517 
Elongation (%) 28 
Reduction in Area (%) 65 
25 water quenched, fine grained, tempered at 650°C   Tensile Strength (MPa) 586 
Yield Strength (MPa) 441 
Elongation (%) 32 
Reduction in Area (%) 70 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.