Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

more free magazines
 
AISI 1040
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
20-100 annealed  11.3 
20-200 annealed  12 
20-300 annealed  12.5 
20-400 annealed  13.3 
20-500 annealed  13.9 
20-600 annealed  14.4 
20-700 annealed  14.8 
20-800 annealed  11.8 
20-1000 annealed  13.6 