Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

more free magazines
 
AISI 1042
ConditionsElectrical Resistivity (10-9W-m)
T (°C)Treatment
20   171 
100   221 
200   296 
400   493 
600   766 
700   932 
800   1111 
900   1149 
1000   1179 
1100   1207 
1200   1230 