Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Resources
Bibliography
Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free magazines
 
AISI 1075
Category Steel
Class Carbon steel
Type Standard
Designations United States: UNS G10750

Composition
ElementWeight %
C  0.70-0.80 
Mn  0.40-0.70 
P  0.04 (max) 
S  0.05 (max) 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  