General Information
Further Details
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
 
AISI 1145
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
0-100 annealed  11.2 
0-200 annealed  12.1 
0-300 annealed  13 
0-400 annealed  13.6 
0-500 annealed  14 
0-600 annealed  14.6 
0-700 annealed  14.8 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.