Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

more free publications
 
AISI 1213
Conditions Tensile Properties 
T (°C)Treatment
25 cold drawn (round bar (19-38 mm))  Tensile Strength (MPa) 540 
Yield Strength (MPa) 415 
Elongation (%) 10 
Reduction in Area (%) 35 
25 hot rolled (round bar (19-38 mm))  Tensile Strength (MPa) 385 
Yield Strength (MPa) 240 
Elongation (%) 25 
Reduction in Area (%) 45 
Glossary
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.