AISI 1215 | |
![]() | |


Conditions | Tensile Properties | ||
T (°C) | Treatment | ||
25 | cold drawn (round bar (19-38 mm)) | Tensile Strength (MPa) | 540 |
Yield Strength (MPa) | 415 | ||
Elongation (%) | 10 | ||
Reduction in Area (%) | 35 | ||
25 | hot rolled (round bar (19-38 mm)) | Tensile Strength (MPa) | 525 |
Yield Strength (MPa) | 470 | ||
Elongation (%) | |||
Reduction in Area (%) | |||
25 | turned and polished (round bar (19-38 mm)) | Tensile Strength (MPa) | 385 |
Yield Strength (MPa) | 230 | ||
Elongation (%) | 25 | ||
Reduction in Area (%) | 45 |