Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
 
AISI 1524
Category Steel
Class Carbon steel
Type Standard
Designations United States: UNS G15240

Composition
ElementWeight %
C  0.19-0.25 
Mn  1.35-1.65 
P  0.04 (max) 
S  0.05 (max) 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 11.9  20-100 more  
Thermal Conductivity (W/m-K) 46  0 more  
Specific Heat (J/kg-K) 477  50-100 more  

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 208  20 more  
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.