AISI 1548
ConditionsHardness
T (°C)TreatmentMethodValue
25 annealed, cold drawn (round bar (19-32 mm))  HB 192 
25 cold drawn (round bar (19-32 mm))  HB 217 
25 hot rolled (round bar (19-32 mm))  HB 197 