Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
World Pumps

Major news, innovation and real-life applications for pumps and ancillary equipment.

NASA Tech Briefs

Innovations developed by NASA and its industry partners in a wide array of fields.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Power Transmission

Gear drives, bearings, motors, clutches, couplings, machine controls, sensors and components.

more free magazines
 
AISI 1045
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
0-100 annealed  11.6 
0-200 annealed  12.3 
0-300 annealed  13.1 
0-400 annealed  13.7 
0-500 annealed  14.2 
0-600 annealed  14.7 
0-700 annealed  15.1 