Specific Cu Alloy
General Information
Resources
Bibliography
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
 
AISI T2
Category Steel
Class Tool steel
Type Tungsten high speed steel
Designations  United States: ASTM A600 , FED QQ-T-590 , SAE J437 , SAE J438 , UNS T12002

Composition
ElementWeight %
C  0.80-0.90 
Mn  0.20-0.40 
Si  0.20-0.40 
Cr  3.75-4.50 
Ni  0.3 
Mo  1.00 (max) 
W  17.50-19.00 
V  1.80-2.40 
Cu  0.25 
P  0.03 
S  0.03 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.67 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Glossary
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.