Specific Cu Alloy
General Information
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
 
UNS C33000
Category Copper Alloy
Class Wrought
Type Low-leaded brass tube
Common Names Copper-zinc brass
Designations United States: UNS C33000

Composition
ElementWeight %
Cu  66.0 
Pb  0.5 
Zn  33.5 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.8-8.94 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 117 25  
Tensile Strength (Mpa) 324-517 25  (tube) more
Yield Strength (Mpa) 103-414
Elongation (%) 60 
Reduction in Area (%)  
Note: Elongation is measured in 7 inches.
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.