Specific Cu Alloy
General Information
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
 
UNS C36500
Category Copper Alloy
Class Wrought
Type Leaded Muntz metal
Common Names Copper-zinc brass
Designations United States: UNS C36500

Composition
ElementWeight %
Cu  60.0 
Pb  0.6 
Zn  39.4 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.8-8.94 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 117 25  
Tensile Strength (Mpa) 372  25  (flat products) 
Yield Strength (Mpa) 138 
Elongation (%) 45 
Reduction in Area (%)  
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.