Metal Alloys
Alloy Home
Copper Alloys
General Information
Properties
Cu Alloy Types
Cast Alloys
Wrought Alloys
Cu Alloy List
UNS C1xxxx
UNS C2xxxx
UNS C3xxxx
UNS C4xxxx
UNS C5xxxx
UNS C6xxxx
UNS C7xxxx
UNS C8xxxx
UNS C9xxxx
Specific Cu Alloy
General Information
Resources
Bibliography
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Hydraulics & Pneumatics

For design and manufacturing engineers involved in buying or specifying fluid power components and systems.

Design-2-Part

How OEM's can make their parts better, faster, and more efficient.

Chemical Engineering

The industry gateway for chemical engineering and plant operations.

more free magazines
 
UNS C43500
Category Copper Alloy
Class Wrought
Common Names Copper-zinc brass
Designations United States: UNS C43500

Composition
ElementWeight %
Cu  81.0 
Sn  0.9 
Zn  18.1 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.8-8.94 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 117 25  
Tensile Strength (Mpa) 317-552 25  (flat products, tube) more
Yield Strength (Mpa) 110-469
Elongation (%) 46 
Reduction in Area (%)  
Note: Elongation is measured in 7 inches.