| UNS C44400 | |
![]() | |
| Conditions | Tensile Properties | ||
| T (°C) | Treatment | ||
| 25 | (flat products, wire, tube) | Tensile Strength (MPa) | 331-379 |
| Yield Strength (MPa) | 124-152 | ||
| Elongation (%) | 65 | ||
| Reduction in Area (%) | |||
| 25 | OS025 (copper alloy tube OD=25 mm, thickness=1.65 mm) | Tensile Strength (MPa) | 365 |
| Yield Strength (MPa) | 150 | ||
| Elongation (%) | 65 | ||
| Reduction in Area (%) | |||