Specific Cu Alloy
General Information
Further Details
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

more free publications
 
UNS C44500
Conditions Tensile Properties 
T (°C)Treatment
25 (flat products, wire, tube)  Tensile Strength (MPa) 331-379
Yield Strength (MPa) 124-152
Elongation (%) 65 
Reduction in Area (%)  
25 OS025 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 365 
Yield Strength (MPa) 150 
Elongation (%) 65 
Reduction in Area (%)  
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.