Metal Alloys
Alloy Home
Copper Alloys
General Information
Properties
Cu Alloy Types
Cast Alloys
Wrought Alloys
Cu Alloy List
UNS C1xxxx
UNS C2xxxx
UNS C3xxxx
UNS C4xxxx
UNS C5xxxx
UNS C6xxxx
UNS C7xxxx
UNS C8xxxx
UNS C9xxxx
Specific Cu Alloy
General Information
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
 
UNS C63000
Category Copper Alloy
Class Wrought
Type Aluminum bronze
Designations United States: UNS C63000

Composition
ElementWeight %
Cu  82.0 
Fe  3.0 
Al  10.0 
Ni  5.0 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.8-8.94 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 117 25  
Tensile Strength (Mpa) 621-814 25  (flat products, rod) 
Yield Strength (Mpa) 345-517
Elongation (%) 20 
Reduction in Area (%)  
Note: Elongation is measured in 15 inches.
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.