Metal Alloys
Alloy Home
Copper Alloys
General Information
Properties
Cu Alloy Types
Cast Alloys
Wrought Alloys
Cu Alloy List
UNS C1xxxx
UNS C2xxxx
UNS C3xxxx
UNS C4xxxx
UNS C5xxxx
UNS C6xxxx
UNS C7xxxx
UNS C8xxxx
UNS C9xxxx
Specific Cu Alloy
General Information
Further Details
Resources
Bibliography
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
 
UNS C65500
Conditions Tensile Properties 
T (°C)Treatment
25 (flat products, rod, wire, tube)  Tensile Strength (MPa) 386-1000
Yield Strength (MPa) 145-483
Elongation (%) 63 
Reduction in Area (%)  
Note: Elongation is measured in 3 inches.
25 H80 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 640 
Yield Strength (MPa)  
Elongation (%) 22 
Reduction in Area (%)  
25 OS050 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 395 
Yield Strength (MPa)  
Elongation (%) 70 
Reduction in Area (%)  
Glossary
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.