Metal Alloys
Alloy Home
Magnesium Alloys
General Information
Properties
Temper
Mg Alloys List
All
Castings
Bars and Shapes
Sheets and Plates
Specific Mg Alloy
General Information
Resources
Bibliography
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

more free publications
 
ASTM AM100A-T61
Category Magnesium Alloy

Composition
ElementWeight %
Al  10.00 
Mn  0.10 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 1.81 25  
Poisson's Ratio 0.35 25  
Elastic Modulus (GPa) 44.8 25  
Tensile Strength (Mpa) 275.0  25  T61 (sand casting, permanent mold casting) 
Yield Strength (Mpa) 150.0 
Elongation (%) 1.0 
Reduction in Area (%)  
Hardness (HB500) 69  25  T61 (sand casting, permanent mold casting) 

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 25.2  18-100 T61 
Thermal Conductivity (W/m-K) 71.13  0  T61 
Glossary
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.