Metal Alloys
Alloy Home
Magnesium Alloys
General Information
Properties
Temper
Mg Alloys List
All
Castings
Bars and Shapes
Sheets and Plates
Specific Mg Alloy
General Information
Resources
Bibliography
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
 
ASTM AZ21X1-F
Category Magnesium Alloy
Designations United States: UNS S44625, ASTM A176, ASTM A276

Composition
ElementWeight %
Al  1.80 
Mn  0.02 
Zn  1.20 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 1.77-1.83 25  
Poisson's Ratio 0.35 25  
Elastic Modulus (GPa) 44.8 25  
Glossary
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.