Metal Alloys
Alloy Home
Magnesium Alloys
General Information
Properties
Temper
Mg Alloys List
All
Castings
Bars and Shapes
Sheets and Plates
Specific Mg Alloy
General Information
Resources
Bibliography
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
 
ASTM AZ31B-H24
Category Magnesium Alloy
Designations United States: UNS N08700, ASTM B599

Composition
ElementWeight %
Al  3.00 
Zn  1.00 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 1.77-1.83 25  
Poisson's Ratio 0.35 25  
Elastic Modulus (GPa) 44.8 25  
Tensile Strength (Mpa) 290.0  25  H24 (sheet, plate) 
Yield Strength (Mpa) 220.0 (180.0) 
Elongation (%) 15.0 
Reduction in Area (%)  
Note: Value in parentheses indicates yield strength for compression.
Hardness (HB500) 73  25  H24 (sheet, plate) 
Shear Strength (MPa) 160  25  H24 (sheet, plate) 

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 26  20-100 H24 
Thermal Conductivity (W/m-K) 96.23  0  H24 
Glossary
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.