| ASTM AZ61A-F | |
![]() | |
| Category | Magnesium Alloy |
| Designations | United States: UNS S44635, ASTM A176 |
| Composition | |
![]() | |
| Mechanical Properties | |
![]() | |
| Properties | Conditions | ||
| T (°C) | Treatment | ||
| Density (×1000 kg/m3) | 1.8 | 25 | |
| Poisson's Ratio | 0.35 | 25 | |
| Elastic Modulus (GPa) | 44.8 | 25 | |
| Tensile Strength (Mpa) | 310.0 | 25 | F (extruded bars and shapes) |
| Yield Strength (Mpa) | 230.0 (130.0) | ||
| Elongation (%) | 16.0 | ||
| Reduction in Area (%) | |||
| Note: Value in parentheses indicates yield strength for compression. | |||
| Hardness (HB500) | 60 | 25 | F (extruded bars and shapes) |
| Shear Strength (MPa) | 140 | 25 | F (extruded bars and shapes) |
| Thermal Properties | |
![]() | |