| ASTM AZ92A-T6 | |
![]() | |
| Category | Magnesium Alloy |
| Designations | United States: UNS S44660, ASTM A176 |
| Composition | |
![]() | |
| Mechanical Properties | |
![]() | |
| Properties | Conditions | ||
| T (°C) | Treatment | ||
| Density (×1000 kg/m3) | 1.82 | 25 | |
| Poisson's Ratio | 0.35 | 25 | |
| Elastic Modulus (GPa) | 44.8 | 25 | |
| Tensile Strength (Mpa) | 275.0 | 25 | T6 (sand casting, permanent mold casting) |
| Yield Strength (Mpa) | 150.0 | ||
| Elongation (%) | 3.0 | ||
| Reduction in Area (%) | |||
| Hardness (HB500) | 84 | 25 | T6 (sand casting, permanent mold casting) |
| Shear Strength (MPa) | 150 | 25 | T6 (sand casting, permanent mold casting) |
| Thermal Properties | |
![]() | |