Metal Alloys
Alloy Home
Magnesium Alloys
General Information
Properties
Temper
Mg Alloys List
All
Castings
Bars and Shapes
Sheets and Plates
Specific Mg Alloy
General Information
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
 
ASTM HZ32A-T5
Category Magnesium Alloy

Composition
ElementWeight %
Th  3.30 
Zn  2.10 
Zr  0.70 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 1.83 25  
Poisson's Ratio 0.35 25  
Elastic Modulus (GPa) 44.8 25  
Tensile Strength (Mpa) 185.0  25  T5 (sand casting, permanent mold casting) 
Yield Strength (Mpa) 90.0 
Elongation (%) 4.0 
Reduction in Area (%)  
Hardness (HB500) 57  25  T5 (sand casting, permanent mold casting) 
Shear Strength (MPa) 140  25  T5 (sand casting, permanent mold casting) 

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 26.7  20-200 T5 
Thermal Conductivity (W/m-K) 108.78  0  T5 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.