Metal Alloys
Alloy Home
Magnesium Alloys
General Information
Properties
Temper
Mg Alloys List
All
Castings
Bars and Shapes
Sheets and Plates
Specific Mg Alloy
General Information
Resources
Bibliography
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
 
ASTM ZH62A-T5
Category Magnesium Alloy

Composition
ElementWeight %
Th  1.80 
Zn  5.70 
Zr  0.70 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 1.86 25  
Poisson's Ratio 0.35 25  
Elastic Modulus (GPa) 44.8 25  
Tensile Strength (Mpa) 240.0  25  T5 (sand casting, permanent mold casting) 
Yield Strength (Mpa) 170.0 
Elongation (%) 4.0 
Reduction in Area (%)  
Hardness (HB500) 70  25  T5 (sand casting, permanent mold casting) 
Shear Strength (MPa) 165  25  T5 (sand casting, permanent mold casting) 

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 27.1  20-200 T5 
Thermal Conductivity (W/m-K) 108.78  0  T5 
Glossary
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.