Metal Alloys
Alloy Home
Magnesium Alloys
General Information
Properties
Temper
Mg Alloys List
All
Castings
Bars and Shapes
Sheets and Plates
Specific Mg Alloy
General Information
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
 
ASTM ZK61A-T5
Category Magnesium Alloy

Composition
ElementWeight %
Zn  6.00 
Zr  0.70 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 1.77-1.83 25  
Poisson's Ratio 0.35 25  
Elastic Modulus (GPa) 44.8 25  
Tensile Strength (Mpa) 310.0  25  T5 (sand casting, permanent mold casting) 
Yield Strength (Mpa) 185.0 
Elongation (%)  
Reduction in Area (%)  
Hardness (HB500) 68  25  T5 (sand casting, permanent mold casting) 
Shear Strength (MPa) 170  25  T5 (sand casting, permanent mold casting) 
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!