Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Further Details
Resources
Bibliography
Hydraulics & Pneumatics

For design and manufacturing engineers involved in buying or specifying fluid power components and systems.

Quality Magazine

Techniques to improve quality on the shop floor and in manufacturing planning.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Design-2-Part

How OEM's can make their parts better, faster, and more efficient.

more free magazines
 
17-4PH
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
0-100   10.8 
0-315   11.6 