TM">
Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
TM">General Information
Further Details
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
 
18-18PlusTM
Conditions Tensile Properties 
T (°C)Treatment
25 annealed (wire)  Tensile Strength (MPa) 635 
Yield Strength (MPa)  
Elongation (%)  
Reduction in Area (%)  
25 annealed (bar)  Tensile Strength (MPa) 760 
Yield Strength (MPa) 415 
Elongation (%) 35 
Reduction in Area (%) 55 
25 annealed (bar)  Tensile Strength (MPa) 825 
Yield Strength (MPa) 450 
Elongation (%) 60 
Reduction in Area (%) 70 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.