Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Further Details
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
 
AISI Type 301
Conditions Tensile Properties 
T (°C)Treatment
25 1/2 hard (sheet, strip)  Tensile Strength (MPa) 1030 
Yield Strength (MPa) 760 
Elongation (%) 18 
Reduction in Area (%)  
25 3/4 hard (sheet, strip)  Tensile Strength (MPa) 1210 
Yield Strength (MPa) 930 
Elongation (%) 12 
Reduction in Area (%)  
25 annealed (bar, wire, plate, sheet, strip)  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%) 40 
Reduction in Area (%)  
25 full hard (sheet, strip)  Tensile Strength (MPa) 1280 
Yield Strength (MPa) 965 
Elongation (%)
Reduction in Area (%)  
25 l/4 hard (sheet, strip)  Tensile Strength (MPa) 860 
Yield Strength (MPa) 515 
Elongation (%) 25 
Reduction in Area (%)  
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.