Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Further Details
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
 
AISI Type 302
Conditions Tensile Properties 
T (°C)Treatment
25 annealed (wire)  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%)  
Reduction in Area (%)  
25 annealed (plate, sheet, strip)  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%) 40 
Reduction in Area (%)  
25 cold finished (wire)  Tensile Strength (MPa) 620 
Yield Strength (MPa) 310 
Elongation (%)  
Reduction in Area (%)  
25 cold finished and annealed (bar (over 13 mm in diameter))  Tensile Strength (MPa) 515 
Yield Strength (MPa)  
Elongation (%)  
Reduction in Area (%) 40 
25 cold finished and annealed (bar (up to 13 mm in diameter))  Tensile Strength (MPa) 620 
Yield Strength (MPa) 310 
Elongation (%) 30 
Reduction in Area (%) 40 
25 high tensile (bar, wire)  Tensile Strength (MPa) 2240 
Yield Strength (MPa)  
Elongation (%)  
Reduction in Area (%)  
25 high tensile, grade B (plate, sheet, strip)  Tensile Strength (MPa) 585 
Yield Strength (MPa) 310 
Elongation (%) 40 
Reduction in Area (%)  
25 high tensile, grade C (plate, sheet, strip)  Tensile Strength (MPa) 860 
Yield Strength (MPa) 515 
Elongation (%)  
Reduction in Area (%)  
25 high tensile, grade D (plate, sheet, strip)  Tensile Strength (MPa) 1030 
Yield Strength (MPa) 760 
Elongation (%)  
Reduction in Area (%)  
25 hot finished and annealed (bar)  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%) 40 
Reduction in Area (%) 50 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.