General Information
Further Details
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
 
AISI Type 303
Conditions Tensile Properties 
T (°C)Treatment
25 annealed (bar)  Tensile Strength (MPa) 585 
Yield Strength (MPa) 240 
Elongation (%) 50 
Reduction in Area (%) 55 
25 annealed (wire)  Tensile Strength (MPa) 585-860
Yield Strength (MPa)  
Elongation (%)  
Reduction in Area (%)  
25 cold worked (wire)  Tensile Strength (MPa) 790-1000
Yield Strength (MPa)  
Elongation (%)  
Reduction in Area (%)  
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!