Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Further Details
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
 
AISI Type 303Se
Conditions Tensile Properties 
T (°C)Treatment
25 annealed   Tensile Strength (MPa) 620 
Yield Strength (MPa) 240 
Elongation (%) 50 
Reduction in Area (%) 55 
25 cold drawn   Tensile Strength (MPa) 690 
Yield Strength (MPa) 415 
Elongation (%) 40 
Reduction in Area (%) 53 
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.