Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
 
AISI Type 304
Category Steel
Class Stainless steel
Type Austenitic standard
Common Names Chromium-Nickel steel
Designations  France: AFNOR Z 6 CN 18.09
Germany: DIN 1.4301
Italy: UNI X 5 CrNi 18 10
Japan: JIS SUS 304
Sweden: SS 2332
United Kingdom: B.S. 302 S 17 , B.S. 304 S 15 , B.S. 304 S 16 , B.S. 304 S 18 , B.S. 304 S 25 , B.S. 304 S 40 , B.S. En.58 E
United States: AMS 5501 , AMS 5513 , AMS 5560 , AMS 5565 , AMS 5566 , AMS 5567 , AMS 5639 , AMS 5697 , ASME SA182 , ASME SA194 (Type 8) , ASME SA213 , ASME SA240 , ASME SA249 , ASME SA312 , ASME SA320 (B8) , ASME SA358 , ASME SA376 , ASME SA403 , ASME SA409 , ASME SA430 , ASME SA479 , ASME SA688 , ASTM A167 , ASTM A182 , ASTM A193 , ASTM A194 , ASTM A213 , ASTM A240 , ASTM A249 , ASTM A269 , ASTM A270 , ASTM A271 , ASTM A276 , ASTM A312 , ASTM A313 , ASTM A314 , ASTM A320 , ASTM A368 , ASTM A376 , ASTM A409 , ASTM A430 , ASTM A473 , ASTM A478 , ASTM A479 , ASTM A492 , ASTM A493 , ASTM A511 , ASTM A554 , ASTM A580 , ASTM A632 , ASTM A651 , ASTM A666 , ASTM A688 , FED QQ-S-763 , FED QQ-S-766 , FED QQ-W-423 , FED STD-66 , MIL SPEC M.IL-S-5059 , MIL SPEC MIL-F-20138 , MIL SPEC MIL-S-23195 , MIL SPEC MIL-S-23196 , MIL SPEC MIL-S-862 , MIL SPEC MIL-S-862 , MIL SPEC MIL-T-6845 , MIL SPEC MIL-T-8504 , MIL SPEC MIL-T-8506 , SAE 30304 , SAE J405 (30304) , UNS S30400

Composition
ElementWeight %
C  0.08 
Mn  2.00 
Si  1.00 
Cr  18.0-20.0 
Ni  8.0-10.5 
P  0.045 
S  0.03 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 193 25  
Tensile Strength (Mpa) 515  25  hot finished and annealed (plate, sheet, strip) more
Yield Strength (Mpa) 205 
Elongation (%) 40 
Reduction in Area (%) 50 
Hardness (HRB) 88  25  annealed (plate, sheet, strip) 

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 17.2  0-100 more  
Thermal Conductivity (W/m-K) 16.2  100 more  
Specific Heat (J/kg-K) 500  0-100   

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 720  25   
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing