Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Further Details
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
 
AISI Type 308
Conditions Tensile Properties 
T (°C)Treatment
25 annealed (plate, sheet, strip)  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%) 40 
Reduction in Area (%)  
25 annealed (wire)  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%)  
Reduction in Area (%)  
25 cold finished (wire)  Tensile Strength (MPa) 620 
Yield Strength (MPa) 310 
Elongation (%)  
Reduction in Area (%)  
25 cold finished and annealed (bar (over 13 mm in diameter))  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%) 30 
Reduction in Area (%) 40 
25 cold finished and annealed (bar (up to 13 mm in diameter))  Tensile Strength (MPa) 620 
Yield Strength (MPa) 310 
Elongation (%) 30 
Reduction in Area (%) 40 
25 hot finished and annealed (bar)  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%) 40 
Reduction in Area (%) 50 
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!