AISI Type 310S | |
Category | Steel |
Class | Stainless steel |
Type | Austenitic standard |
Common Names | Chromium-Nickel steel |
Designations | United States: AMS 5521 , AMS 5572 , AMS 5577 , AMS 5651 , ASME SA240 , ASME SA479 , ASTM A167 , ASTM A240 , ASTM A276 , ASTM A314 , ASTM A473 , ASTM A479 , ASTM A511 , ASTM A554 , ASTM A580 , SAE 30310S , SAE J405 (30310S) |
Composition | |
Mechanical Properties | |
Properties | Conditions | ||
T (°C) | Treatment | ||
Density (×1000 kg/m3) | 7.7-8.03 | 25 | |
Poisson's Ratio | 0.27-0.30 | 25 | |
Elastic Modulus (GPa) | 190-210 | 25 | |
Tensile Strength (Mpa) | 515 | 25 | hot finished and annealed (wire) more |
Yield Strength (Mpa) | 205 | ||
Elongation (%) | 40 | ||
Reduction in Area (%) | 50 | ||
Hardness (HRB) | 95 (max) | 25 | annealed (plate, sheet, strip) |
Thermal Properties | |