Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Further Details
Resources
Bibliography
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
 
AISI Type 316N
Conditions Tensile Properties 
T (°C)Treatment
25 annealed (plate, sheet, strip)  Tensile Strength (MPa) 550 
Yield Strength (MPa) 240 
Elongation (%) 30 
Reduction in Area (%)  
25 annealed (bar)  Tensile Strength (MPa) 550 
Yield Strength (MPa) 240 
Elongation (%) 30 
Reduction in Area (%)  
25 annealed (bar)  Tensile Strength (MPa) 550 
Yield Strength (MPa) 240 
Elongation (%) 30 
Reduction in Area (%)  
Glossary
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.