Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Further Details
Resources
Bibliography
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
 
AISI Type 317
Conditions Tensile Properties 
T (°C)Treatment
25 annealed (wire)  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%)  
Reduction in Area (%)  
25 annealed (plate, sheet, strip)  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%) 35 
Reduction in Area (%)  
25 cold finished (wire)  Tensile Strength (MPa) 620 
Yield Strength (MPa) 310 
Elongation (%)  
Reduction in Area (%)  
25 cold finished and annealed (bar (over 13 mm in diameter))  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%) 30 
Reduction in Area (%) 40 
25 cold finished and annealed (bar (up to 13 mm in diameter))  Tensile Strength (MPa) 620 
Yield Strength (MPa) 310 
Elongation (%) 30 
Reduction in Area (%) 40 
25 hot finished and annealed (bar)  Tensile Strength (MPa) 515 
Yield Strength (MPa) 205 
Elongation (%) 40 
Reduction in Area (%) 50 
Glossary
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.