Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Further Details
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
 
AISI Type 404
Conditions Tensile Properties 
T (°C)Treatment
25 tempered at 260°C (bar)  Tensile Strength (MPa) 1120 
Yield Strength (MPa) 910 
Elongation (%) 15 
Reduction in Area (%) 50 
25 tempered at 595°C (bar)  Tensile Strength (MPa) 745 
Yield Strength (MPa) 655 
Elongation (%) 23 
Reduction in Area (%) 70 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.