Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Further Details
Resources
Bibliography
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
 
AISI Type 410Cb
Conditions Tensile Properties 
T (°C)Treatment
25 annealed, cold finished (bar)  Tensile Strength (MPa) 485 
Yield Strength (MPa) 275 
Elongation (%) 12 
Reduction in Area (%) 35 
25 annealed, hot finished (bar)  Tensile Strength (MPa) 485 
Yield Strength (MPa) 275 
Elongation (%) 13 
Reduction in Area (%) 45 
25 intermediate temper, cold finished (bar)  Tensile Strength (MPa) 860 
Yield Strength (MPa) 690 
Elongation (%) 12 
Reduction in Area (%) 35 
25 intermediate temper, hot finished (bar)  Tensile Strength (MPa) 860 
Yield Strength (MPa) 690 
Elongation (%) 13 
Reduction in Area (%) 45 
Glossary
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.