Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Resources
Bibliography
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
 
AISI Type 414
Category Steel
Class Stainless steel
Type Martensitic standard
Common Names Chromium steel
Designations  United States: AMS 5615 , ASTM A276 , ASTM A314 , ASTM A473 , ASTM A511 , ASTM A580 , FED QQ-S-763 , SAE 51414 , SAE J405 (51414) , UNS S41400

Composition
ElementWeight %
C  0.15 
Mn  1.00 
Si  1.00 
Cr  11.5-13.5 
Ni  1.25-2.50 
P  0.04 
S  0.03 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.8 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 200 25  
Tensile Strength (Mpa) 1030  25  annealed, cold finished (wire) more
Yield Strength (Mpa)  
Elongation (%)  
Reduction in Area (%)  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 10.4  0-100 more  
Thermal Conductivity (W/m-K) 24.9  100 more  
Specific Heat (J/kg-K) 460  0-100   

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 700  25   
Glossary
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.