| AISI Type 414 | |
![]() | |
| Conditions | Tensile Properties | ||
| T (°C) | Treatment | ||
| 25 | annealed, cold finished (wire) | Tensile Strength (MPa) | 1030 |
| Yield Strength (MPa) | |||
| Elongation (%) | |||
| Reduction in Area (%) | |||
| 25 | intermediate temper, cold finished (bar) | Tensile Strength (MPa) | 795 |
| Yield Strength (MPa) | 620 | ||
| Elongation (%) | 15 | ||
| Reduction in Area (%) | 45 | ||
| 25 | intermediate temper, hot finished (bar) | Tensile Strength (MPa) | 795 |
| Yield Strength (MPa) | 620 | ||
| Elongation (%) | 15 | ||
| Reduction in Area (%) | 45 | ||