AISI Type 633 | |
![]() | |


Conditions | Tensile Properties | ||
T (°C) | Treatment | ||
25 | annealed | Tensile Strength (MPa) | 1105 |
Yield Strength (MPa) | 415 | ||
Elongation (%) | 30 | ||
Reduction in Area (%) | |||
25 | double aged | Tensile Strength (MPa) | 1180 |
Yield Strength (MPa) | 980 | ||
Elongation (%) | 12 | ||
Reduction in Area (%) | |||
25 | subzero cooled and tempered at 455°C | Tensile Strength (MPa) | 1365 |
Yield Strength (MPa) | 1115 | ||
Elongation (%) | 15 | ||
Reduction in Area (%) | 49 | ||
25 | subzero cooled and tempered at 540°C | Tensile Strength (MPa) | 1125 |
Yield Strength (MPa) | 1035 | ||
Elongation (%) | 22 | ||
Reduction in Area (%) | 53 |