Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Further Details
Resources
Bibliography
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
 
AISI Type 634
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
25-100   17.1 
25-200   18.1 
25-310   18.4 
25-400   18.9 
25-500   19.3 
25-600   19.8 
25-1000   20.3 
Glossary
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.