Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Further Details
Resources
Bibliography
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

more free publications
 
AISI Type 635
Conditions Tensile Properties 
T (°C)Treatment
25 H1000 (bar, plate, sheet, strip)  Tensile Strength (MPa) 1240 
Yield Strength (MPa) 1100 
Elongation (%)
Reduction in Area (%) 30 
25 H1050 (bar, plate, sheet, strip)  Tensile Strength (MPa) 1170 
Yield Strength (MPa) 1070 
Elongation (%) 10 
Reduction in Area (%) 40 
25 H950 (bar, plate, sheet, strip)  Tensile Strength (MPa) 1310 
Yield Strength (MPa) 1170 
Elongation (%)
Reduction in Area (%) 25 
Glossary
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.