| Nitronic50 | |
![]() | |
| Category | Steel |
| Class | Stainless steel |
| Type | Austenitic nonstandard |
| Composition | |
![]() | |
| Element | Weight % |
| C | 0.06 |
| Mn | 4.0-6.0 |
| Si | 1.00 |
| Cr | 20.5-23.5 |
| Ni | 11.5-13.5 |
| P | 0.0 |
| S | 0.03 |
| Mo | 1.5-3.0 |
| N | 0.2-03 |
| Nb | 0.1-0.3 |
| V | 0.1-0.3 |
| Mechanical Properties | |
![]() | |
| Nitronic50 | |
![]() | |
| Category | Steel |
| Class | Stainless steel |
| Type | Austenitic nonstandard |
| Composition | |
![]() | |
| Element | Weight % |
| C | 0.06 |
| Mn | 4.0-6.0 |
| Si | 1.00 |
| Cr | 20.5-23.5 |
| Ni | 11.5-13.5 |
| P | 0.0 |
| S | 0.03 |
| Mo | 1.5-3.0 |
| N | 0.2-03 |
| Nb | 0.1-0.3 |
| V | 0.1-0.3 |
| Mechanical Properties | |
![]() | |

Optimize your designs, reduce machining time, and lower your costs.
Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.
Guide for high quality and cost-effective plastic injection molding.
Wages, employment opportunities, and growth projections for STEM jobs.