| Found 4 records |
Titanium Alloy

| Name | Purpose | Grade |
| Ti-11.5Mo-6Zr-4.5Sn | Wrought | Beta alloy |
| Ti-13V-11Cr-3Al | Wrought | Beta alloy |
| Ti-3Al-8V-6Cr-4Mo-4Zr | Wrought | Beta alloy |
| Ti-8Mo-8V-2Fe-3Al | Wrought | Beta alloy |
| Found 4 records |

| Name | Purpose | Grade |
| Ti-11.5Mo-6Zr-4.5Sn | Wrought | Beta alloy |
| Ti-13V-11Cr-3Al | Wrought | Beta alloy |
| Ti-3Al-8V-6Cr-4Mo-4Zr | Wrought | Beta alloy |
| Ti-8Mo-8V-2Fe-3Al | Wrought | Beta alloy |