Metal Alloys
Alloy Home
Titanium Alloys
General Information
Properties
Ti Alloys List
All
Commercially Pure
Alpha Alloys
Near Alpha Alloys
Alpha-Beta Alloys
Beta Alloys
Specific Ti Alloy
General Information
Further Details
Resources
Bibliography
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

more free publications
 
99.5 Ti
Conditions Tensile Properties 
T (°C)Treatment
25 annealed   Tensile Strength (MPa) 331 
Yield Strength (MPa) 241 
Elongation (%) 30 
Reduction in Area (%) 55 
315 annealed   Tensile Strength (MPa) 152 
Yield Strength (MPa) 97 
Elongation (%) 32 
Reduction in Area (%) 80 
Glossary
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.