Metal Alloys
Alloy Home
Titanium Alloys
General Information
Properties
Ti Alloys List
All
Commercially Pure
Alpha Alloys
Near Alpha Alloys
Alpha-Beta Alloys
Beta Alloys
Specific Ti Alloy
General Information
Further Details
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
 
Ti-7AI-4Mo
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
20-100   9 
20-205   9.2 
20-315   9.4 
20-425   9.7 
20-540   10.1 
20-650   10.4 
20-815   11.2 
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.